carbonear59
Mechanical
we have a piece of A106 B pipe that has damage on the bevelled end . we are working under B31.3 Normal Service ,
where would i look to find the appropriate code section
that allows me to 'butter ' the bevelled end to correct the gap before welding the joint ?
thanks
where would i look to find the appropriate code section
that allows me to 'butter ' the bevelled end to correct the gap before welding the joint ?