Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Degree of cure Test Requirement

Status
Not open for further replies.

makhawaja

Mechanical
Mar 21, 2015
1
Guys...
Can ayone guide me on below querie.

Degree of cure can be done generally on Epoxy Finished Products painting system
Since our Painting system is polyurethane finished, it is not desirable to do degree of cure on this.

Degree of cure test can be done for polyurethane finished paint system or not.
 
Replies continue below

Recommended for you

Degree of cure can be done on essentially any class of coating. One difficulty is defining the cure criteria for the specific coating.

Google Dwight Weldon. He is a coating and materials consultant in Pennsylvania. He has provided consulting to me on several coatings issues and he's very good.
 