Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Depth of sawcuts

Status
Not open for further replies.

federicop

Materials
Dec 17, 2008
1
How relative is the depth of saw cut relative to the concrete thickness and the timing of the sawcut to receive caulk material?

 
Replies continue below

Recommended for you

Missed this... but the depth should be 1/4 to 1/3 of the slab thickness and should occur approx 6hrs to 8hrs after finishing. Can be sooner with a sofcut type of saw