I need to apply dimensional tolerances to drawings of composite parts used in aircraft interiors. These are mouldings and fabrications using cut and fold techniques. Does anyone know of any standards that could be applied ?
First shouldn't you look at what tolerances are needed based on functionality then verify if your proposed production technique/material can meet them?