Divider plate welded column splice

Status
Not open for further replies.

bvsiq

Structural
Aug 4, 2007
6
To transition from a 13l4" square x 1/2" HSS to a 12"square x 1/2" HSS, thinking of using a 3/4" divider plate, butt welded to 14" column and then 7/16" fillet weld upper col to divider plate- what do you guys think?
 
Replies continue below

Recommended for you

It sounds fine, especially if it's a shop splice. Obviously, the plate and the welds need to be designed for the real load effects acting on the connection. That said, the proportions of what you've proposed seem pretty stout so it's hard to imagine that you'll have any trouble.