Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Does anyone know resistivity value of ........

Status
Not open for further replies.

tor2k

Electrical
May 5, 2005
2
Does anyone know resistivity value of road base(class 2)?
 
Replies continue below

Recommended for you

This may varies widely considering the aggregate contain binder soil and fines. Probably someone in this forum could help if more detail is provided regarding the composition of the class 2 material or just measuring soil sample(s)

If I have to guess, the wet resistivity may be 400 to 1000 Ohm-m.
 