abourandas
Chemical
- Sep 26, 2008
- 3
API 571 says that wet H2S damage occurs from ambient to 300F. My example is an HOC reactor effluent line at 1655 PSI and 424F going to a High Pressure Hot Seperator. Will wet H2S be a concern at this high of a temperature since the pressure will keep the water in the liquid phase?