Gents

Is it permissable to use a Dolly-mix (Vertical up GTAW / SMAW - Vertical Down) Groove PQR in P1 Group 1 (Without notch toughness)to perform a vertical groove weld? Code is ASME IX, with no application standards

Thanks
 
Replies continue below

Recommended for you

The WPS could have been qualified in the flat (1G) position.