Nov 8, 2015 #1 Ingenuity Structural May 17, 2001 2,373 Has any one used or have experience with this DRADER INJECTIWELD plastic welding unit? Link My application is 2.0mm thick HDPE tubing of 16mm diamater where I wish to weld a longitudinal seam.
Has any one used or have experience with this DRADER INJECTIWELD plastic welding unit? Link My application is 2.0mm thick HDPE tubing of 16mm diamater where I wish to weld a longitudinal seam.
Nov 9, 2015 1 #2 ornerynorsk Industrial Feb 5, 2002 3,198 You might consider sending them a sample and asking them to perform a weld on it to demonstrate their machine's capability. It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all. Upvote 0 Downvote
You might consider sending them a sample and asking them to perform a weld on it to demonstrate their machine's capability. It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
Nov 10, 2015 Thread starter #3 Ingenuity Structural May 17, 2001 2,373 Thanks, ornerynorsk, excellent idea. Star for you! Upvote 0 Downvote
Nov 22, 2015 Thread starter #4 Ingenuity Structural May 17, 2001 2,373 By way of follow-up, I sent a sample to one of the manufacturer's resellers and they conducted a trial weld and returned the sample to me: Upvote 0 Downvote
By way of follow-up, I sent a sample to one of the manufacturer's resellers and they conducted a trial weld and returned the sample to me: