Sep 8, 2011 #1 MSSandvik Materials May 24, 2010 9 0 0 SE Does anyone know if there are any standard drill point geometries for CFRP drilling? By this i mean NAS 907 describes some drills and the metals they're to be used on. Is there one for CFRP? Any help appreciated
Does anyone know if there are any standard drill point geometries for CFRP drilling? By this i mean NAS 907 describes some drills and the metals they're to be used on. Is there one for CFRP? Any help appreciated
Sep 8, 2011 #2 rerig Aerospace Aug 6, 2003 286 0 0 US Page 19 http://files.engineering.com/getfile.aspx?folder=9f5458f5-3677-4785-9d3c-85facb373ed2&file=6M62-656_Machining_Plastics_and_Advanced_Composites.pdf Upvote 0 Downvote
Sep 9, 2011 Thread starter #3 MSSandvik Materials May 24, 2010 9 0 0 SE rerig Nice one, this looks good. I assume the ST10-907-A is a NAS 907 A point geomtery? Thanks for your help. Upvote 0 Downvote
rerig Nice one, this looks good. I assume the ST10-907-A is a NAS 907 A point geomtery? Thanks for your help.