Hello friends
Duplex steel 2205 , thickness 7/8", not heat treated, Exemption from Notch toughness test, 100% Radiography on butt weld joints.
do Ferratic testing & Liquid Penetrant is that mandatory.
please advice.
Regards
stan
 
Replies continue below

Recommended for you

What is your code of construction for the tank?????
 