materialpinar
Materials
Dear all,
I have a question about Duplex steel(2205) production in induction furnaces. This is my master topic . The company I work for does not want to work with refined ingot, so we will work with 316 L.
Can I clean the furnaces with bottom-dipping argon?
is there anything I can measure the nitrogen in the mine?
where should I start working from ?
can anyone help step by step to create a chemical with 316 l?
thank you very much in advance.
I have a question about Duplex steel(2205) production in induction furnaces. This is my master topic . The company I work for does not want to work with refined ingot, so we will work with 316 L.
Can I clean the furnaces with bottom-dipping argon?
is there anything I can measure the nitrogen in the mine?
where should I start working from ?
can anyone help step by step to create a chemical with 316 l?
thank you very much in advance.