Sep 17, 2010 #1 rmob970 New member Feb 23, 2009 1 0 0 CA Has anyone used EC2216 as liquid shim? Any compressive strength data on EC2216 that may be available would be helpful
Has anyone used EC2216 as liquid shim? Any compressive strength data on EC2216 that may be available would be helpful
Sep 20, 2010 #2 rerig Aerospace Aug 6, 2003 286 0 0 US I wouldn't recommend EC2216 for liquid shim. BMS 5-92 doesn't have compressive nor density. We have used EA934 (Dexter-Hysol) for liquid shim applications. http://files.engineering.com/getfile.aspx?folder=ff188fff-5ef7-4436-b8b0-3f128f71247d&file=EC-2216_Issue_No._4.pdf Upvote 0 Downvote
I wouldn't recommend EC2216 for liquid shim. BMS 5-92 doesn't have compressive nor density. We have used EA934 (Dexter-Hysol) for liquid shim applications.
Sep 20, 2010 #3 rerig Aerospace Aug 6, 2003 286 0 0 US EA934 http://files.engineering.com/getfile.aspx?folder=b0c20f36-94b1-44e3-ac83-2210856d1d15&file=EA_934NA.pdf Upvote 0 Downvote