KimWonGun
Mechanical
- Oct 11, 2010
- 78
I am trying to find an economical way to continuously dispense a 2K urethane. My ideal is using a recirculating valve, but the cost of that valve --- along with a manifold and handle --- is about $1,400 from Nordson (450RC).
Since this is a development program, I am not keen to invest that sum at present and ask if anyone knows of either a more competitive supplier or another dispensing method that allows continuous material flow while controlling shut-off at the mixer?
Since this is a development program, I am not keen to invest that sum at present and ask if anyone knows of either a more competitive supplier or another dispensing method that allows continuous material flow while controlling shut-off at the mixer?