In the standart composition of Hadfield steel the phosphorus contents are max 0,07% wt. I'm finding hard to find information of the efects of these percentage of phosphorus in this alloy.Is there a way of reducing phosphorus content?
 
Replies continue below

Recommended for you

If you are having arc furnace melting,then it is possible to further reduce P content. In induction furnace practice, the final P will remain unchanged. You must carefully select your charge.

I have not come across any failure due to high P content as long as it in within limits..