GGEFAB
Petroleum
- Apr 17, 2003
- 2
What effect will stress relieving 2.25%Cr 1%Mo material at 1200F for 1.5 hours have on hardness in the HAZ after welding if we extend the cooldown period. Will it increase the hardness or decrease the hardness.