silence1
Materials
- Sep 7, 2005
- 1
I would like to do the modeling of elastomer (compression) with Marc software. But I just have uniaxial tension and compression test results of the elastomer. And there is the problem of fitting the parameter in the model. I use Mooney-Rivlin model. But the parameter after data fitting becomes negative (C10 or C01 becomes negative). This then cause errors in the modeling.
Can anyone tell me which model will be best for this kind of modeling? How to slove the parameter problem?
Can anyone tell me which model will be best for this kind of modeling? How to slove the parameter problem?