Apr 8, 2020 #1 Raza Rauf Mechanical Apr 4, 2020 9 0 0 PK Hello Reader, Which electrode to be used for welding grey cast iron with API5L? Moreover, please share the reference for future. Thanks!
Hello Reader, Which electrode to be used for welding grey cast iron with API5L? Moreover, please share the reference for future. Thanks!
Apr 8, 2020 #2 Dhurjati Sen Materials Dec 14, 2017 948 0 0 IN The non-standard (but effective) practice is to use inconel electrode. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Apr 8, 2020 #3 Tmoose Mechanical Apr 12, 2003 5,626 0 0 US Is this a structural weld? Successful cast iron welding requires much more than just a suitable electrode. Have you found information like this ? - https://www.lincolnelectric.com/en-...-detail.aspx?utm_referrer=direct/not+provided Upvote 0 Downvote
Is this a structural weld? Successful cast iron welding requires much more than just a suitable electrode. Have you found information like this ? - https://www.lincolnelectric.com/en-...-detail.aspx?utm_referrer=direct/not+provided
Apr 8, 2020 #4 arunmrao Materials Oct 1, 2000 4,758 0 0 IN Any high Nickel(>55%), is usually used. But I have not had much success. Upvote 0 Downvote
Apr 8, 2020 #5 weldstan Materials Jun 24, 2011 2,730 0 36 US This is gray iron? Forget about it!! It could be brazed. If ductile iron, a high nickel filler can be used. Upvote 0 Downvote
This is gray iron? Forget about it!! It could be brazed. If ductile iron, a high nickel filler can be used.
Apr 9, 2020 #7 EdStainless Materials May 20, 2004 15,893 0 36 US If you have pieces to sacrifice then try welding. Otherwise look into brazing. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy Upvote 0 Downvote
If you have pieces to sacrifice then try welding. Otherwise look into brazing. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy
Apr 10, 2020 #8 0707 Petroleum Jun 25, 2001 3,327 0 0 PT if it was white cast iron it will be non weldable. luis marques Upvote 0 Downvote