I am looking to get a part Electroless Nickel plated to approximately 0.002-0.0025" thick. The part is an aluminum casting, not sure of the alloy. The inside diameter of the area to be plated is approximately 2.4". The manual specifies MIL-C-26074. Is this thickness easily attainable?

Part 2: Is it possible to machine the electroless nickel coating to a good finish and hold a tolerance of 0.0007" (total) or does it need to be ground?
 
Replies continue below

Recommended for you

Depends on what you're making. People have diamond turned electroless nickel for optics, but that usually requires a post-polish.