May 4, 2003 #1 bslgeoff Chemical Nov 26, 2002 3 0 0 AU Hello Everybody Just seeking info on whether anybody out there know of some tin mills that use direct application of oil? Also if I could be directed to a website explaining ESI and how temperature effects can be determined. Thanks Geoff
Hello Everybody Just seeking info on whether anybody out there know of some tin mills that use direct application of oil? Also if I could be directed to a website explaining ESI and how temperature effects can be determined. Thanks Geoff
May 5, 2003 #2 25362 Chemical Jan 5, 2003 4,826 0 0 CA If by ESI you mean emulsion stability index then by asking just that phrase from the internet you may find a lot of articles dealing with the subject. The same regarding colloidal mills. Good luck! Upvote 0 Downvote
If by ESI you mean emulsion stability index then by asking just that phrase from the internet you may find a lot of articles dealing with the subject. The same regarding colloidal mills. Good luck!