Hello all,
I'm looking for some guidance regarding a welding qualification: I am looking to qualify EN 10025-6:2019 S690QL. The customer specification lists some quite demanding mechanical testing, though the one I'm worried about is the NACE hardness acceptance requirements, plus the customers additional cruciform hardness.
Looking through EN 10025-6 however I can't see any limit on hardness for S690. Can anyone advise where this may be stated - I know it will be on the material certification though it hasn't been ordered yet, and I'm aware there may be a caveat for materials as-received that are already above the hardness requirements.
Thanks
I'm looking for some guidance regarding a welding qualification: I am looking to qualify EN 10025-6:2019 S690QL. The customer specification lists some quite demanding mechanical testing, though the one I'm worried about is the NACE hardness acceptance requirements, plus the customers additional cruciform hardness.
Looking through EN 10025-6 however I can't see any limit on hardness for S690. Can anyone advise where this may be stated - I know it will be on the material certification though it hasn't been ordered yet, and I'm aware there may be a caveat for materials as-received that are already above the hardness requirements.
Thanks