Can somebody tell me what is the EN equivalent of SAE 4340
 
Replies continue below

Recommended for you

If EN means Euronorm, then there is no exact equivalent standard grade. EN 10083-1 has two grades that are similar: 36CrNiMo4 (1.6511) and 36NiCrMo16 (1.6773). There are many heat-treatable grades of steel that contain Cr, Ni, and Mo, and usually you can choose a satisfactory alternative based on the requirements for strength, hardenability, toughness, etc. If you provide additional details about the part and its requirements, we can assist you further.
 