deco0404
Mechanical
- Nov 3, 2009
- 79
Hi guys,
Im doing a couple of jobs at the moment using some strange steel designations that I am not entirely familiar with....
Does anyone have or know where to get a full list of designations for EN Steels.ie, exactly what each designation means!
I am talking specifically about the prefix letters
J - specific impact values
N- Normalised
Q- Quenched
T- Tempered
etc............
On a more urgent note, if someone could tell me what the 'D' in S355D is. We think it is hot-dip coated....
Thanks,
Declan
Im doing a couple of jobs at the moment using some strange steel designations that I am not entirely familiar with....
Does anyone have or know where to get a full list of designations for EN Steels.ie, exactly what each designation means!
I am talking specifically about the prefix letters
J - specific impact values
N- Normalised
Q- Quenched
T- Tempered
etc............
On a more urgent note, if someone could tell me what the 'D' in S355D is. We think it is hot-dip coated....
Thanks,
Declan