- May 16, 2009
- 4
I have an existing 5' X 10' X 4" pad that is too small. I don't want to have to chip it up to pour the new pad. The new pad will be about 6' X 20'. I plan on stippling the top of the old pad with a chipping hammer and coating it with an epoxy bonding agent. I need the finished pad to be at least 6" thick. Is 2" of concrete on top of the old pad going to be enough? Or should I make it thicker? Any other suggestions? The equipment going on the pad will weigh about 2,500 pounds.