fabrication of alloy 625 and Alloy 718

Status
Not open for further replies.

will123123

Materials
Nov 26, 2009
46
We have a component that is a fabrication of both alloy 625 and alloy 718, due to the need for different requirement in certain areas. Some parts need higher strength where as others parts will be subjected to high temperatures (+900°C). Currently this is heat treated after manufacture using the standard solution treatment and ageing process for 718. Could anyone tell me the likely implications for the mechanical properties and durability of alloy 625?

 