roberthathaway
Materials
- Oct 22, 2008
- 8
We use a 5/16" thick 110 ksi min. yield hss material formed into a rectangle and resistance welded to form a frame rail. A pair of these tubes combined with cross members makes up a chassis. We are experiencing localized fracture in the throat of the weld initiating at the weld crown. Starts ductile and goes brittle. Looking at 350 Knoop hardness in the fusion zone. Has anyone experience such a failure?