Dear all,

We have a high strength vessel, UTS is between 86 ksi-93 ksi in cyclic service. But Div 2, Fig 3-F does not have a curve for such UTS. Where can I find one ?
 
Replies continue below

Recommended for you

Per 3-F.1.2(a)
ASME Section VIII said:
... The fatigue curve values may be interpolated for intermediate values of the ultimate tensile strength.
 