All,

It appears this has been brought up in years past but none of the referenced links seem to work. Much like our trustworthy DOS based Ferrite software does to not like modern advancements in Windows...

Does anyone know of any online or purchasable programs that will predict Ferrite? Out of the many advancements in the formula we rely on the WRC method.

Thanks
 
I have found a few on the web that seem to work fine.
I haven't gone to any great lengths to validate them though.
I'll look for the links and post them later.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
May be I am too late to help you over this.
Gone through a welding software, Weldpulse including Ferrite prediction. It uses WRC 1992 diagram. I have verified the result to one example in AWS publication.