working in the gulf area where the temp exceeds 50c.
for garage workshop and parking building.

I am required to approve the contractor mix design for the above subject.

his design as follows:
W/C ratio : 0.51
Slump: 125mm
Cement: 410 Kg/m3
0-5 crushed sand : 1280kg/m3
Dune Sand: 410kg/m3
admixture: CF-100 (Sodap)
any help in this matter will be appreciated.

Wadid Lotfy
Structural Engineer
Dubai, UAE
 