Hi,
I am looking for the cost difference between a coating system providing corrosion protection and a coating system providing besides corrosion protection also fire protection.
Hence I have the following questions.
1) What would be a typical system providing corrosion protection only ? and what would be its all-in/applied rate in USD/m2 ?
2) Same questions but now for a typical system also providing fire protection for a duraion of 2 hrs (e.g. Chartek 7)
thanks, Theo van Adrichem
I am looking for the cost difference between a coating system providing corrosion protection and a coating system providing besides corrosion protection also fire protection.
Hence I have the following questions.
1) What would be a typical system providing corrosion protection only ? and what would be its all-in/applied rate in USD/m2 ?
2) Same questions but now for a typical system also providing fire protection for a duraion of 2 hrs (e.g. Chartek 7)
thanks, Theo van Adrichem