Not having access to the 2003 B16.5, can someone tell me what the allowable pressure rating is for a 300 pound flange at a temperature of 300F?

Thanks
 
Replies continue below

Recommended for you

From B16.5 2003 a material group 1.1 (which includes A-105) CL-300 flange at 300 deg F has a pressure rating of 655 psi. Don't forget to leave some margin for piping loads (tensile longitudinal and moments) which will act with the internal pressure to open up the flange.