I am in desperate need of a ceramic to use in a head gasket setting.
I have used Macor with the thousand little pieces after it was run for 20 minutes. I think it actually broke up when we un-torqued the head. (no carbon in the cracks)
we tried aluminum oxide and it broke radially with no particular pattern.
Next we were looking into silicon nitride but it is costly and difficult to find a grinder to put in some 1mm holes that we need.
Thanks in advance for your help
ref:US patent 7299785
I don't know anything but the people that do.