Aug 15, 2008 #1 wilburfhh Mechanical May 3, 2006 12 0 0 US A quick tank question, API 650, 653. If you have to repair a weld on the Flush Cleanout type fittings, which it has been already stress relieved, Do you have to stress relieve it again once you do the repair? Let me know. Thanks a lot.
A quick tank question, API 650, 653. If you have to repair a weld on the Flush Cleanout type fittings, which it has been already stress relieved, Do you have to stress relieve it again once you do the repair? Let me know. Thanks a lot.
Aug 16, 2008 #2 JoeTank Structural Oct 28, 1999 1,133 0 0 US API has passed a revision to the Standard that uses a pre-heat alternative to re-PWHT. Contact API (http://www.API.org) to obtain a copy of it. Joe Tank Upvote 0 Downvote
API has passed a revision to the Standard that uses a pre-heat alternative to re-PWHT. Contact API (http://www.API.org) to obtain a copy of it. Joe Tank