Hello,

We are using some 6" dia., 0.5" thick Duro50 and Duro70 (Shore A) Neoprene pads for various boundary conditions on a test structure in our lab. We have already performed force vs. displacement plots using our UTM (to obtain pad vertical stiffness values) and were looking for some published/manufacturer plots (or values) to compare with. I posted this question in here since we are using the same pads that are used for typ. concrete cylinder tests, hoping someone might have some info. or suggestions.