Forgings in ASTM A105 normalised at -20¦F (-29¦C)

Status
Not open for further replies.

federella

Mechanical
May 19, 2005
12
0
0
IT
Some studies have demonstrated that about 40% of Main Flanges in ASTM A105, despite the certificates, have not been treated properly after forging and that the transition temperature, with a mean impact toughness, of 27J is about + 20°C.
The question is how is possible that ANSI/ASME B16.34 authorized to employ this forging at - 29°C taking also in account the aggravating point that the mechanical properties can be verified with specimen obtained from separated forged test blanks (as per ASTM A105)?
 
Replies continue below

Recommended for you

I guess it all boils down to reputable forging suppliers. Most users specify low temp material for anything less than -29C although ASME VIII can give impact test exemption down to -55F (-48C). I personally would not recommend impact testing A105, rather switch to A350-LF2.
 