Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

formable alloy steel sheet recommendation

Status
Not open for further replies.

mechengdude

Mechanical
Mar 6, 2007
209
If anyone could recommend material(s) to meet the following requirements, it would be appreciated:
1. Steel
2. Must be formable (90 degree bend max)
3. 50Ksi yield minimum
4. Corrosion resistance is a non-factor
5. Cost not a hard requirement but cheaper is better
7. Thickness range approximately .050"

Regards
 
Replies continue below

Recommended for you

HSLA steels are probably the lowest cost option for this strength range. Official designation is either HSLAS Grade 50 according to ASTM A1011 or 340X according to SAE J2340.
 