Dear sir,

If we see the TWI- Job knoweldge 103, there is table as shown below.
Table 1 Typical compositions of some austenitic stainless steel alloys

ASTM No.
(type) Composition wt% Microstructure
C (max) Si (max) Mn (max) Cr Ni Mo Others Austenite - A
Ferrite - F
304 0.08 0.75 2.0 18/20 8/11 - - A+2/8%F
304L 0.035 0.75 2.0 18/20 8/11 - - A + 2/8%F
304H 0.04 - 0.10 0.75 2.0 18/20 8/11 - - A + 2/8%F
304N 0.08 0.75 2.0 18/20 8/11 - 0.1/0.16N A + 2/8%F
316 0.08 0.75 2.0 16/18 11/14 2/3 - A + 3/10%F
347 0.08 0.75 2.0 17/20 9/13 - Nb : 10xC A + 4/12%F
321 0.08 0.75 2.0 17/19 9/12 - Ti: 5xC A + 4/12%F
310 0.15 0.75 2.0 24/26 19/22 - - 100% A
309 0.08 1.0 2.0 22/24 12/15 - - A + 8/15%F
308L (generally filler metal only) 0.03 1.0 2.0 19/21 10/12 A + 4/12%F

In this table what is meant by 2/8 % F- i know that F is delta ferrtie , only want to know what is 2/8 and why 316L material not shown in table.
Any special reason behind the not showing such common usable material 316L.

Pls giude
Regards
Prasad rode
 
Replies continue below

Recommended for you

Thanks for the clarify about ferrite phase range.

But why they not shown 316L, however, shown 304, 304L, 304H, 304N.

Why not 316L. Any special reason?