Feb 9, 2024 #1 Sathya R Mechanical Nov 6, 2023 2 0 0 IN How to design and size the bracket support in FRP tank. Any reference for design calculations?
Feb 12, 2024 #2 EdClymer Mechanical Jan 15, 2003 100 0 16 GB Sathya R Not much information in your question. For FRP (or GRP in Europe) implying a glass and resin structure the design codes are BS4994 and ASME RTP-1. As an alternative (not helpful) try EN13121. What was the tank originally designed to? Brackets can be designed by FEA based on data gleaned from a standard ie stain, stress and Modulus. Trust this helps. Ed Clymer Resinfab & Associates England Upvote 0 Downvote
Sathya R Not much information in your question. For FRP (or GRP in Europe) implying a glass and resin structure the design codes are BS4994 and ASME RTP-1. As an alternative (not helpful) try EN13121. What was the tank originally designed to? Brackets can be designed by FEA based on data gleaned from a standard ie stain, stress and Modulus. Trust this helps. Ed Clymer Resinfab & Associates England