Hi,
Problem: Internal damaged galvanizing due to welding
Proposal: Because of extent of damage area is very small magnitude compare with the over-all length the contractor
recommended that:-
1) if the location is near by open end such as flanges, galvanized paint shall be applied internally as practicable
2) if distanced from such open end, then damaged repair shall be made on outer surface only
Any opinion/advise on the above recommendation?
ppm
Problem: Internal damaged galvanizing due to welding
Proposal: Because of extent of damage area is very small magnitude compare with the over-all length the contractor
recommended that:-
1) if the location is near by open end such as flanges, galvanized paint shall be applied internally as practicable
2) if distanced from such open end, then damaged repair shall be made on outer surface only
Any opinion/advise on the above recommendation?
ppm