Taoufik Sbai
Automotive
Hello
For an automotive application, i have to set the boundary acceptance for dross / dross inclusions per unit surface area.
The only input that I found for says med dross less than 2mm are acceptable (Surface EUC 7 Standard) without referring to any quantity.
I will appreciate any guidance for this topic
Thanks
For an automotive application, i have to set the boundary acceptance for dross / dross inclusions per unit surface area.
The only input that I found for says med dross less than 2mm are acceptable (Surface EUC 7 Standard) without referring to any quantity.
I will appreciate any guidance for this topic
Thanks