Jun 26, 2007 #1 amanites Mechanical Mar 23, 2007 21 0 0 BE I need to select a suitable gasket to be used in a pipeline transporting either soya/rapeseed oil or biodiesel.Any advice please.
I need to select a suitable gasket to be used in a pipeline transporting either soya/rapeseed oil or biodiesel.Any advice please.
Jun 27, 2007 #2 shi2shi Chemical Dec 7, 2006 3 0 0 GB Hi amanites in order of suitability: Furon PTFE coated rubber Goretex Viton hope this helps. Upvote 0 Downvote
Jun 29, 2007 #3 DYV1973 Mechanical Aug 9, 2004 75 0 0 NL Do not use EPDM or something similar. Viton or NBR might be okay. If you use rubber with a PTFE around it, please note that the PTFE will deform when pressed together, so it can not be used for connections that need to be opened every now and then. Upvote 0 Downvote
Do not use EPDM or something similar. Viton or NBR might be okay. If you use rubber with a PTFE around it, please note that the PTFE will deform when pressed together, so it can not be used for connections that need to be opened every now and then.