Hello everybody,
A pressure control globe valve made of carbon steel (SCH 160,CS ASTM A106 GRB) has been
severely corroded in a gas plant,this valve is placed in between two pipes (SMLS,ASME B36.10M,
BE END, SCH 160, CS ASTM A106 GRB)assembled by a spiral wound gasket (GSKT SPRL WND ASME
B16.20 ASME B16.5 CL 600,TP304, SS WDG, Graphite Flr,TP 304, SS INR RING,CS OTR RING).
THis valve has been changed by another valve which has the same design only made by Stainless
steel instead of Carbon Steel.
my question is how to connect (gasket type) a pipe made by a Carbon steel with Stsainless
steel valve?
i believe that the gasket mentioned above is not suitable for this assemblage due to the
electrochemical potential caused by contactig the inner ring (SS)to a Pipe flange made by (CS)
any help would be appreciate,
Best regards,
Adem
A pressure control globe valve made of carbon steel (SCH 160,CS ASTM A106 GRB) has been
severely corroded in a gas plant,this valve is placed in between two pipes (SMLS,ASME B36.10M,
BE END, SCH 160, CS ASTM A106 GRB)assembled by a spiral wound gasket (GSKT SPRL WND ASME
B16.20 ASME B16.5 CL 600,TP304, SS WDG, Graphite Flr,TP 304, SS INR RING,CS OTR RING).
THis valve has been changed by another valve which has the same design only made by Stainless
steel instead of Carbon Steel.
my question is how to connect (gasket type) a pipe made by a Carbon steel with Stsainless
steel valve?
i believe that the gasket mentioned above is not suitable for this assemblage due to the
electrochemical potential caused by contactig the inner ring (SS)to a Pipe flange made by (CS)
any help would be appreciate,
Best regards,
Adem