Aug 6, 2020 #1 amper Electrical Oct 3, 2008 52 0 0 GB sr hi can anyone with experience recomended the best sustitute for old asbestos gasket sheet with tinplate used in the burning chamber injectors .
sr hi can anyone with experience recomended the best sustitute for old asbestos gasket sheet with tinplate used in the burning chamber injectors .
Sep 1, 2020 #2 DAVIDSTECKER Mechanical Mar 23, 2005 525 0 0 US Look at the high temp gasket material at McMaster-Carr. Upvote 0 Downvote