manuvarier
Marine/Ocean
The rotor winding of one of our genset in our DP vessel twice failed because of the rotor winding gets cut after few days of operation. Both times, the winding gets cut at different location of the winding.The genset rotor was overhauled, rewinded, baked , rotor balanced, refitted and tested 2 mths back . A major maintenance was carried out then. Since then, after few odays of operation the genset was out of order because at one location the rotor winding was cut and there was no continiuty. The wires were reconnected by soildering and tested , all seemed ok. We continued running the genset after temporary repair for few days , the genset brokes down again because of the rotor winding got cut at a different location..
Please suggest , what could be the major cause of this faults recurring , what is the best solution to avoid such break downs.
Please suggest , what could be the major cause of this faults recurring , what is the best solution to avoid such break downs.