For Demin water stator cooling system
Why is the conductivity lower coming back from the generator then going to the generator.
Going to gen after HX and IX is about 0.13 micro Siemen/cm
Coming back from gen is about 0.5 micro Siemen/cm
Temp coming back is about 60 degree C
Temp going to gen is about 47 degree C
Why is the conductivity lower coming back from the generator then going to the generator.
Going to gen after HX and IX is about 0.13 micro Siemen/cm
Coming back from gen is about 0.5 micro Siemen/cm
Temp coming back is about 60 degree C
Temp going to gen is about 47 degree C