SteelBloke
Industrial
- Apr 17, 2003
- 7
I personally wouldn't cut bisalloy on a gillotine which is capable of cutting 6mm stainless, but a boily mate said he had and did it was about 5mm and i did'nt see the grade but you could hear it crackling as it was cut and sounded like a glass crunching sound, is this wise?.