I am looking for a adhesive / glue which is used to bond staple pins (all kinds) during production process. An ideal glue should be less viscous (thin), transparent liquid. It should provide a very strong bond at a temerature around 50 to 60 degrees centrigrade. It should be corrosion resistant. It should also provide a liqour / shiny finish.

More over staple pins should not seperate from each other under ordinary circumstances for very long period. Could some one guide me how could I find it? How can I classify it?
 