Dec 30, 2014 #1 GunnyD Automotive May 25, 2006 6 0 0 US What spec covers the grain flow pattern for cold formed rivets.
Dec 31, 2014 #2 CoryPad Materials Apr 15, 2002 5,192 0 0 US SAE/USCAR-8 Grain Flow Pattern for Bolts, Screws, and Studs is an example standard but not specific to rivets. Upvote 0 Downvote
SAE/USCAR-8 Grain Flow Pattern for Bolts, Screws, and Studs is an example standard but not specific to rivets.