GRE limitations

Status
Not open for further replies.

KMur

Mechanical
Apr 27, 2007
40
Dear ALL,
Where can I get the GRE limitaions in terms of pressure and temperaure? Please advise sutiable standards.
Thanks
 
Replies continue below

Recommended for you

The pressure and temperature limitations come from the manufacturer supported by the required qualification test documentation that may be as per API Spec 15HR, ASME X, or ISO 14692-2 amongst others.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 