Obviously answers to this question will be somewhat turbine specific, but I am after a ball park figure.
What percentage of the total air mass flow rate through the compressor is extracted for use cooling the bucket internal passages?
I have heard reference to 1-2% per stage, which is believable, but also reference to 10%+ per stage.